THE TRANSFORMATION OF AMORPHOUS CALCIUM CARBONATE TO CALCITE IN THE PRESENCE OF STRONTIUM
Paper number: T155-6
Program: Technical Sessions
Time: 9:10 AM – 9:25 AM
Authors
-
Juliane WeberOak Ridge National Laboratory, Oak Ridge, TN
-
Joanne StubbsUniversity of Chicago, Chicago, IL
-
Peter J. EngUniversity of Chicago, Chicago, IL
-
Tyler L. SpanoOak Ridge, TN
-
Tingting LiuOak Ridge National Laboratory, Oak Ridge, TN
-
Bryan ChakoumakosOak Ridge National Laboratory, Oak Ridge, TN
-
Hsiu-Wen WangRichmond, TX
-
Andrew G. StackOak Ridge National Laboratory, Oak Ridge, TN
Abstract
Sr2+-free ACC materials with stoichiometry of Ca1.000(OH)0.098(CO3)0.951·1.246H2O were synthesized and confirmed by thermogravimetric analysis and X-ray diffraction (XRD). To study the Sr2+ incorporation effects during ACC to calcite transformation, 200 mg of Sr-free ACC powers were mixed in 20 mL SrCl2 solution with Sr2+ concentration varied from 0-0.1M at 25oC in batch reactors. The solid end products were analyzed ex-situ with SEM-EDS, XRD, and Raman spectroscopy for every 5, 10, 30, 180, and 1440 minutes. When the initial Sr2+ concentration is higher than 0.8 mM (i.e., Sr/Ca > 0.01), a mixture of calcite and strontianite (SrCO3) is formed. When Sr2+ concentration is less than 0.8 mM (i.e., Sr/Ca < 0.01), the final product is found to be a single phase of calcite, but with up to 10 wt.% Sr in replacement of Ca in the calcite structure. This latter observation can be explained by dissolution and reprecipitation reactions in which ACC dissolves first and reprecipitates to form Sr-rich calcite. In addition, the crystallinity and crystal morphology of calcite are affected by the enrichment of Sr2+ in the initial solution. For instance, with higher Sr2+ concentration, calcite developed more multi-twinned crystals and reduced crystallinity visible in peak broadening of Raman spectra. Significant Raman peak shift of the C-O in-plane bending mode around 712 cm-1 and rotational mode around 280 cm-1 to the lower frequencies is observed, which suggests positional disorder of carbonate ions and induced-lattice strains due to the Sr2+ to Ca2+ substitution. Details about kinetics and crystallographic changes during ACC to calcite transformations will be studied in the near future by in-situ time-resolved synchrotron XRD methods.
Geological Society of America Abstracts with Programs. Vol. 54, No. 6
doi: 10.1130/abs/2022AM-379185
© Copyright 2022 The Geological Society of America (GSA), all rights reserved. Permission is hereby granted to the author(s) of this abstract to reproduce and distribute it freely, for noncommercial purposes. Permission is hereby granted to any individual scientist to download a single copy of this electronic file and reproduce up to 20 paper copies for noncommercial purposes advancing science and education, including classroom use, providing all reproductions include the complete content shown here, including the author information. All other forms of reproduction and/or transmittal are prohibited without written permission from GSA Copyright Permissions.